ASTM D2462-1990(2001) Standard Test Method for Moisture in Wool by Distillation With Toluene《用甲苯蒸馏法测定羊毛中水分的试验方法》.pdf
《ASTM D2462-1990(2001) Standard Test Method for Moisture in Wool by Distillation With Toluene《用甲苯蒸馏法测定羊毛中水分的试验方法》.pdf》由会员分享,可在线阅读,更多相关《ASTM D2462-1990(2001) Standard Test Method for Moisture in Wool by Distillation With Toluene《用甲苯蒸馏法测定羊毛中水分的试验方法》.pdf(5页珍藏版)》请在麦多课文档分享上搜索。
1、Designation: D 2462 90 (Reapproved 2001)Standard Test Method forMoisture in Wool by Distillation With Toluene1This standard is issued under the fixed designation D 2462; the number immediately following the designation indicates the year oforiginal adoption or, in the case of revision, the year of l
2、ast revision. A number in parentheses indicates the year of last reapproval. Asuperscript epsilon (e) indicates an editorial change since the last revision or reapproval.1. Scope1.1 This test method covers the determination of the amountof moisture present in grease wool, scoured wool, carded wool,g
3、arnetted wool, wool top and intermediate wool products, androvings, by distillation with toluene.1.2 Equations are given for calculating the amount of waterpresent as moisture content (as-received basis) and moistureregain (dry fiber) basis. The term that corresponds to the basisused in the calculat
4、ion and report must always be stated.1.3 This test method is not applicable to material known tocontain any steam-distillable, water-soluble matter. If it issuspected that such matter is present, the method should beused with caution.1.4 Xylene or other solvents should not be substituted fortoluene
5、as no other solvents have been evaluated for use in thisstandard.NOTE 1The determination of moisture in wool by oven-drying iscovered in Test Method D 1576 and for textile materials in general in TestMethods D 2654. A method for sampling wool for the determination ofmoisture in wool is covered in Pr
6、actice D 2525.1.5 This standard does not purport to address all of thesafety concerns, if any, associated with its use. It is theresponsibility of the user of this standard to establish appro-priate safety and health practices and determine the applica-bility of regulatory limitations prior to use.
7、For specific safetyhazard statements, see Section 8.2. Referenced Documents2.1 ASTM Standards:D 123 Terminology Relating to Textiles2D 1060 Practice for Core Sampling of Raw Wool in Pack-ages for Determination of Percentage of Clean Wool FiberPresent2D 1576 Test Method for Moisture in Wool by Oven-D
8、rying2D 1776 Practice for Conditioning Textiles for Testing2D 2258 Practice for Sampling Yarn for Testing2D 2495 Test Method for Moisture in Cotton by Oven-Drying2D 2525 Practice for Sampling Wool for Moisture2D 2654 Test Methods for Moisture in Textiles2D 3333 Practice for Sampling Man-Made Staple
9、Fibers,Sliver, or Tow for Testing3E 123 Specification for Apparatus for Determination ofWater by Distillation43. Terminology3.1 Definitions:3.1.1 grease wool, n.wool taken from the living sheep andwhich has not been commercially scoured.3.1.2 moisture content, n.the amount of moisture in amaterial d
10、etermined under prescribed conditions and expressedas a percentage of the mass of the moist material, that is, theoriginal mass comprising the oven-dried substance plus anymoisture present.3.1.2.1 DiscussionThe term “mass” is the correct desig-nation for the property commonly designated as “weight.”
11、 Aslight amount of residual moisture may not be removed from aspecimen subjected to oven drying because of the relativehumidity of the ambient air. The amount of moisture retainedby a specimen may be estimated from published data. Theremay also be a slight additional loss in mass caused by theevapor
12、ation of volatile material other than water, the amountdepending on the characteristics of any added oils or emul-sions.3.1.3 moisture-free, adj.the condition of a material thathas been exposed in an atmosphere of desiccated air until thereis no further significant change in its mass (see Discussion
13、under 3.1.2)3.1.3.1 DiscussionHeating the material and the desiccatedair to temperatures as high as 110C increases the rate ofmoisture loss but does not change the final equilibrium mass ofthe moisture-free material.3.1.4 moisture regain, n.the amount of moisture in amaterial determined under prescr
14、ibed conditions and expressedas a percentage of the mass of the moisture-free material (seemoisture content).3.1.4.1 DiscussionIn this test method, the material isconsidered to be oven-dried after drying as described inSection 10.3.1.5 oven-dried, adj.the condition of a material that hasbeen heated
15、under prescribed conditions of temperature and1This test method is under the jurisdiction of ASTM Committee D13 on Textiles,and is the direct responsibility of Subcommittee D13.13 on Wool and Wool Felt.Current edition approved Aug. 31, 1990. Published October 1990. Originallypublished as D 246266. L
16、ast previous edition D 2462 77 (1983).2Annual Book of ASTM Standards, Vol 07.01.3Annual Book of ASTM Standards, Vol 07.02.4Annual Book of ASTM Standards, Vol 14.02.1Copyright ASTM, 100 Barr Harbor Drive, West Conshohocken, PA 19428-2959, United States.humidity until there is no further significant c
17、hange in its mass(see 3.1.2).3.1.5.1 DiscussionAn oven-dried material will retain asmall amount of moisutre which is dependent on the tempera-ture and relative humidity of the atmosphere in contact with thematerial during the drying process. An oven-dried material willonly be moisture-free when the
18、air supplied to the drying ovenhas been previously desiccated.3.1.6 pulled wool, n.wool taken from the pelt of aslaughtered sheep and which has not been commerciallyscoured. (syn. slipe wool, skin wool).3.1.7 raw wool, n.wool or hair of the sheep in the grease,pulled, or scoured state. (See also sco
19、ured wool.)3.1.8 recycled wool, n.as defined in the Wool ProductsLabeling Act as amended in 1980, “the resulting fiber whenwool has been woven or felted into a wool product which,without ever having been utilized in any way by the ultimateconsumer, subsequently has been made into a fibrous state, or
20、the resulting fiber when wool or reprocessed wool has beenspun, woven, knitted, or felted into a wool product which, afterhaving been used in any way by the ultimate consumer,subsequently has been made into a fibrous state.”3.1.8.1 DiscussionIn the amended Act of 1980, the term“recycled wool” replac
21、ed the terms “reprocessed wool” and“reused wool.”3.1.9 scoured wool, n.wool from which the bulk ofimpurities has been removed by an aqueous or solvent washingprocess.3.1.9.1 DiscussionAlthough it is no longer in its originalraw state, scoured wool is generally accepted as raw wool.3.1.10 virgin wool
22、, n.as defined in the Wool ProductsLabeling Act, “the terms 8virgin or 8new as descriptive of awool product, or any fiber or part thereof, shall not be usedwhen the product or part so described is not composed whollyof new or virgin fiber which has never been reclaimed from anyspun, woven, knitted,
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
10000 积分 0人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- ASTMD246219902001STANDARDTESTMETHODFORMOISTUREINWOOLBYDISTILLATIONWITHTOLUENE 甲苯 蒸馏 测定 羊毛 水分 试验 方法 PDF

链接地址:http://www.mydoc123.com/p-512904.html