ASTM D4245-2008(2013) Standard Specification for Ozone-Resistant Thermoplastic Elastomer Insulation For Wire and Cable 90° C Dry 75° C Wet Operation《工作温度为90℃干 75℃湿的电线和电缆的耐臭氧热.pdf
《ASTM D4245-2008(2013) Standard Specification for Ozone-Resistant Thermoplastic Elastomer Insulation For Wire and Cable 90° C Dry 75° C Wet Operation《工作温度为90℃干 75℃湿的电线和电缆的耐臭氧热.pdf》由会员分享,可在线阅读,更多相关《ASTM D4245-2008(2013) Standard Specification for Ozone-Resistant Thermoplastic Elastomer Insulation For Wire and Cable 90° C Dry 75° C Wet Operation《工作温度为90℃干 75℃湿的电线和电缆的耐臭氧热.pdf(2页珍藏版)》请在麦多课文档分享上搜索。
1、Designation: D4245 08 (Reapproved 2013) An American National StandardStandard Specification forOzone-Resistant Thermoplastic Elastomer Insulation ForWire and Cable, 90C Dry/75C Wet Operation1This standard is issued under the fixed designation D4245; the number immediately following the designation i
2、ndicates the year oforiginal adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. Asuperscript epsilon () indicates an editorial change since the last revision or reapproval.1. Scope*1.1 This specification covers an ozone-res
3、istant insulatingcompound for electrical wire and cables 14 AWG and larger.This compound consists substantially of a thermoplastic elas-tomer.1.2 This type of insulation is suitable for continuous opera-tion at conductor temperatures not exceeding 90C in drylocations and 75C in wet locations. Operat
4、ing voltages are notto exceed 2000 V. The minimum installation temperatureis 40C.1.3 The values stated in inch-pound units are to be regardedas standard. The values given in parentheses are mathematicalconversions to SI units that are provided for information onlyand are not considered standard.1.4
5、In many instances the insulation material cannot betested unless it has been formed around a conductor or cable.Therefore, tests are done on insulated wire or cable in thisdocument solely to determine the relevant property of theinsulation material and not to test the conductor or completedcable.2.
6、Referenced Documents2.1 ASTM Standards:2D470 Test Methods for Crosslinked Insulations and Jacketsfor Wire and CableD1711 Terminology Relating to Electrical InsulationD2633 Test Methods for Thermoplastic Insulations andJackets for Wire and Cable3. Terminology3.1 Definitions: For definitions of terms
7、used in this speci-fication refer to Terminology D1711.3.2 Definitions of Terms Specific to This Standard:3.2.1 aging, nexposure of materials to air at 121 C for168 h.4. Physical Properties4.1 Requirements for physical properties are listed in Table1.4.2 Thickness of InsulationTable 1A (Conductor Si
8、zes,Insulation Thicknesses, and AC Test Voltages for RubberInsulations) of Test Methods D470 lists the minimum averagethickness for the insulation. The required minimum thicknessis 90 % of the specified average thickness.5. Electrical Requirements5.1 Order of TestingPerform the ac voltage withstand
9、test,insulation resistance, and dc voltage withstand test in that orderwhen any of these tests are specified. The sequence of othertesting is not specified.5.2 AC Voltage Withstand TestUnless otherwise specified,omit this test if the dc voltage withstand test described in 5.4 isto be performed. Test
10、 each insulated conductor for 5 min at theac withstand voltage given in Table 1A (Conductor Sizes,Insulation Thicknesses, and AC Test Voltages for RubberInsulations) of Test Methods D470 under the columns labeled“Ozone-Resisting Insulation.”5.3 Insulation Resistance5.3.1 The insulated conductor shal
11、l have an insulationresistance value of at least that corresponding to a constant of10 000 at 60F (15.6C).5.3.2 If the water temperature at the time measurement wasmade differs from 60F (15.6C), correct the insulation resis-tance to 60F. Table 2, (Temperature Correction Factors forInsulation Resista
12、nce at 60F), of Test Methods D470, containsthe correction factors. Use the procedure given in Test MethodsD470 to determine the 1F coefficient for the insulationmaterial. Multiply the measured value by the correction factorto obtain the insulation resistance value corrected to 60F.5.3.3 If the insul
13、ated conductor is covered with a non-metallic sheath so that the insulation resistance can be mea-sured only on the completed assembly, the required insulationresistance shall be not less than 60 % of that required for theprimary insulation based on the thickness of that insulation.1This specificati
14、on is under the jurisdiction of ASTM Committee D09 onElectrical and Electronic Insulating Materials and is the direct responsibility ofSubcommittee D09.18 on Solid Insulations, Non-Metallic Shieldings and Coveringsfor Electrical and Telecommunication Wires and Cables.Current edition approved Nov. 1,
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
10000 积分 0人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- ASTMD424520082013STANDARDSPECIFICATIONFOROZONERESISTANTTHERMOPLASTICELASTOMERINSULATIONFORWIREANDCABLE90DEGCDRY75DEGCWETOPERATION

链接地址:http://www.mydoc123.com/p-516628.html