FORD WSS-M11P62-A-2007 ADHESIVE INTERIOR PERFORMANCE TO BE USED WITH FORD WSS-M99P1111-A 《汽车内部用胶粘剂的性能 与标准FORD WSS-M99P1111-A一起使用 》.pdf
《FORD WSS-M11P62-A-2007 ADHESIVE INTERIOR PERFORMANCE TO BE USED WITH FORD WSS-M99P1111-A 《汽车内部用胶粘剂的性能 与标准FORD WSS-M99P1111-A一起使用 》.pdf》由会员分享,可在线阅读,更多相关《FORD WSS-M11P62-A-2007 ADHESIVE INTERIOR PERFORMANCE TO BE USED WITH FORD WSS-M99P1111-A 《汽车内部用胶粘剂的性能 与标准FORD WSS-M99P1111-A一起使用 》.pdf(4页珍藏版)》请在麦多课文档分享上搜索。
1、 ENGINEERING MATERIAL SPECIFICATION Date Action Revisions 2007 06 18 Revised Inserted 3.0; Deleted 3.1, 3.2, 3.3, 3.11, 3.12 & 4 1999 02 10 Revised Revised 3.6 & 3.8.1 L. Koth 1996 07 03 Activated L. Koth Printed copies are uncontrolled Copyright 2007, Ford Global Technologies, LLC Page 1 of 4 ADHES
2、IVE, INTERIOR PERFORMANCE WSS-M11P62-A 1. SCOPE This specification defines the performance requirements for adhesives used in interior applications. 2. APPLICATION This specification was released originally for adhesives used to manufacture interior assemblies and/or subassemblies, (i.e. door trim,
3、consoles, headliners, carpet laminates, etc.) 3. REQUIREMENTS 3.0 STANDARD REQUIREMENTS FOR PRODUCTION MATERIALS Material suppliers and part producers must conform to the Companys Standard Requirements For Production Materials (WSS-M99P1111-A). 3.4 FLAMMABILITY, max 100 mm/min (ISO 3795/SAE J369) Fo
4、r adhesives that are bonded over 100% of substrate surface area: Test sample preparation: Prepare composite sample with production substrates and adhesive. The adhesive thickness, application, and cure methods must reproduce the production process. Exceptions to this method require prior approval an
5、d written concurrence from the appropriate Materials Engineer. For adhesives having point-contact with the substrate (e.g. hot melt): Test sample preparation: Apply the adhesive film to a suitable release liner. The adhesive thickness, application, and cure methods must reproduce the production proc
6、ess. Remove the release liner for testing. Exceptions to this method require prior approval and written concurrence from the appropriate Materials Engineer. 3.5 ODOR, max 2 rating (SAE J 1351) Test sample preparation: Apply the adhesive to aluminum foil. The adhesive thickness, application and cure
7、methods must reproduce the production process. 3.6 FOGGING (SAE J1756, 3 h at 100 C heating, 21 C cooling plate, post test conditioning 1 h and 16 h) Fog Number, min 70 Formation of clear film, droplets or crystals is cause for rejection. ENGINEERING MATERIAL SPECIFICATION WSS-M11P62-A Printed copie
8、s are uncontrolled Copyright 2007, Ford Global Technologies, LLC Page 2 of 4 Test sample preparation: Apply the adhesive to aluminum foil. The adhesive thickness, application and cure methods must reproduce the production process. Exceptions to this method require prior approval and written concurre
9、nce from the appropriate Materials Engineer. 3.7 STORAGE STABILITY, min 90 days When stored in sealed unopened containers out of direct sunlight at ambient temperatures between 5 and 32 C. 3.8 ADDITIONAL LINE CALLOUT REQUIREMENTS All callout digits shall be specified on the engineering drawing and a
10、pproved source list. Create an 8 digit line callout to further characterize the adhesive using the classification system below. *All “As specified“ (Z) digits must be defined in the supplier submission, on the engineering drawing and approved source list. 3.8.1 First Digit Reference specification fo
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
10000 积分 0人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- FORDWSSM11P62A2007ADHESIVEINTERIORPERFORMANCETOBEUSEDWITHFORDWSSM99P1111A 汽车 内部 胶粘剂 性能 标准 FORDWSSM99P1111A

链接地址:http://www.mydoc123.com/p-751209.html