ASTM F1454-1999(2003) Standard Practice for Comparing Correctable Film Ribbons《可改正的薄膜色带比较的标准规范》.pdf
《ASTM F1454-1999(2003) Standard Practice for Comparing Correctable Film Ribbons《可改正的薄膜色带比较的标准规范》.pdf》由会员分享,可在线阅读,更多相关《ASTM F1454-1999(2003) Standard Practice for Comparing Correctable Film Ribbons《可改正的薄膜色带比较的标准规范》.pdf(5页珍藏版)》请在麦多课文档分享上搜索。
1、Designation: F 1454 99 (Reapproved 2003)Standard Practice forComparing Correctable Film Ribbons1This standard is issued under the fixed designation F 1454; the number immediately following the designation indicates the year oforiginal adoption or, in the case of revision, the year of last revision.
2、A number in parentheses indicates the year of last reapproval. Asuperscript epsilon (e) indicates an editorial change since the last revision or reapproval.1. Scope1.1 This practice provides information and techniques forevaluating performance qualities of a correctable film ribbon. Itcan be used to
3、 evaluate typewriter ribbons for general officeuse.1.2 The values stated in either SI or inch-pound units are tobe regarded as the standard. The values given in parenthesesare for information only.1.3 This standard does not purport to address all of thesafety concerns, if any, associated with its us
4、e. It is theresponsibility of the user of this standard to establish appro-priate safety and health practices and determine the applica-bility of regulatory limitations prior to use.2. Referenced Documents2.1 ASTM Standards:2D 685 Practice for Conditioning Paper and Paper Productsfor TestingD 882 Te
5、st Methods for Tensile Properties of Thin PlasticSheetingD 3460 Specification for White Watermarked, Unwater-marked Bond, Mimeograph, Duplicator, and ZerographicCut-Sized Office PapersF 497 Practice for Use of the Electric and Electronic Type-writer as a Test InstrumentF 1050 Test Method for Determi
6、ning Winding Torque andTension of Typewriter RibbonsF 1125 Terminology of Image Quality in Impact PrintingSystemsF 1174 Practice for Using a Personal Computer as a TestInstrumentF 1443 Practice for Using 0.008-in. (0.023-mm) ApertureReflectometers as Test Instruments for Measuring VisualImage Qualit
7、y of Business Copy Images3. Terminology3.1 DefinitionsFor terms that are used in this practice, seeTerminology F 1125.4. Summary of Practice4.1 This practice covers testing for physical properties ofcorrectable film ribbons, performance testing of correctablefilm ribbons under actual and simulated c
8、onditions on type-writers, and using the results to determine a comparative rating.All sample ribbons and supplies should be conditioned andtested under identical conditions in order to obtain comparativeresults.4.2 All sample ribbons may be tested and compared withknown control ribbons, a previous
9、set of data, or an establishedstandard.5. Significance and Use5.1 This practice should be used to evaluate performancequalities of correctable film ribbons on a comparative basisunder actual and simulated conditions.5.2 This practice is suitable for comparative service evalu-ation, research, and dev
10、elopment. It may also be used formanufacturing quality control.5.3 Users may choose any one test, a series of tests, or alltests, depending on their needs and interests in determining thedifferent characteristics of correctable film ribbons.6. General Considerations6.1 The following statements addre
11、ss some concerns aboutquality of the product. Although a complete list is not provided,the user must make the final determination of performancecriteria factors and level at which each factor impacts theparticular analysis.6.2 Visual InspectionInspect the ribbon for a smooth,uniform coating (on the
12、appropriate film base) free of folds,wrinkles, splices, blisters, uncoated areas, cracks, contamina-tion, and other detrimental defects that would make the ribbonunfit for its intended purpose. Examine for a smoothly slitstraight edge and proper winding without ragged and nickededges.1This practice
13、is under the jurisdiction of ASTM Committee F05 on BusinessImaging Products and is the direct responsibility of Subcommittee F05.02 on InkedRibbons and Carbon Paper.Current edition approved July 10, 1999. Published September 1999. Originallypublished as F 1454 - 94. Last previous edition F 1454 94.2
14、For referenced ASTM standards, visit the ASTM website, www.astm.org, orcontact ASTM Customer Service at serviceastm.org. For Annual Book of ASTMStandards volume information, refer to the standards Document Summary page onthe ASTM website.1Copyright ASTM International, 100 Barr Harbor Drive, PO Box C
15、700, West Conshohocken, PA 19428-2959, United States.6.3 Ribbon Winding Examine and report telescoping orlayer slippage that may have occurred in handling of the woundand assembled ribbon cartridges.6.4 Ribbon Cassette Design and performance of a ribboncassette may be compared to a control product o
16、r otherestablished standard. Inspect the cassette for dirt, oil, or anyother type of debris that may cause functional or aestheticproblems.7. Apparatus and Materials7.1 Electronic Typewriter or Printer, capable of being set upin accordance with Practice F 497.7.2 Microdensitometer or Reflectance Met
17、er, equipped witha 0.008-in. (0.203-mm) aperture and grid pattern in accordancewith Practice F 1443.7.3 Environmental Chamber, capable of maintaining 120 62.0F (49 6 0.16C) for 48 h at a relative humidity of 50 62%.7.4 Type Font, capable of producing a printed image with astroke width exceeding 0.00
18、8 in. (0.203 mm).7.5 Paper, which may be the grade normally used in thefacility conducting the test or the grade conforming withSpecification D 3460, Grade 1 or 4, Type I Bond, Basis 20 or24 lb (9 or 11 kg).8. Conditioning8.1 The test specimen, equipment, and paper should beconditioned in accordance
19、 with Practice D 685.9. Test Methods9.1 WeightFrom positions approximately 50 ft (15 m)apart on the ribbon spool, cut five 1 m 6 1-mm lengths.Determine weight of each to 0.001 g and report the average.9.2 Base Thickness Using the five samples from theribbon weight test, remove the entire coating wit
20、h a suitablesolvent, air dry, and measure the thickness in two places foreach sample. Report the average thickness to 0.0001 in.(0.0025 mm) or better.9.3 Tensile Properties:9.3.1 This test is in accordance with Test Methods D 882,using the following conditions:9.3.1.1 Sample Dimensions6.0 in. (152 m
21、m) long.9.3.1.2 Cross Head Speed 20.00 in. (508 mm)/min.9.3.1.3 Chart Speed 5.00 in. (127 mm)/min.9.3.1.4 Jaw Separation 2.00 in. (51 mm).9.3.2 Report the following:9.3.2.1 Ribbon/leader/trailer tensile strength at yield,9.3.2.2 Ribbon/leader/trailer tensile strength at break, and9.3.2.3 Ribbon/lead
22、er/trailer percent elongation at yield andbreak.9.4 Ribbon Dimensions:9.4.1 Measure the ribbon width, length, and pancake diam-eter by means of tape measure and calipers.9.4.2 Measure the leader/trailer width and length by meansof tape measure and calipers.9.5 Visual Reflectance of Image:9.5.1 Appar
23、atus:9.5.1.1 Typewriter or Printer, to be used as a test instrumentset to manufacturers specifications.9.5.1.2 Model 082 Clearwave Optical Character Tester3orequivalent equipment, set to visual reflectance.9.5.1.3 Type Font, of style and size desired, set at mediumimpression.9.5.1.4 Typing Paper, of
24、 the style and type desired.9.5.1.5 Test Conditions506 2 % relative humidity and73 6 2F (236 0.16C).9.5.2 Procedure:9.5.2.1 Turn on the Clearview Model 082 or equivalentinstrument, and allow it to stabilize for at least12 h. Zero themachine in accordance with the manufacturers instructions.Place cal
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
5000 积分 0人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- ASTMF145419992003STANDARDPRACTICEFORCOMPARINGCORRECTABLEFILMRIBBONS 改正 薄膜 色带 比较 标准规范 PDF

链接地址:http://www.mydoc123.com/p-534920.html