ANSI AWS D18.2-2009 GUIDE TO WELD DISCOLORATION LEVELS ON INSIDE OF AUSTENITIC STAINLESS STEEL TUBE (Abstract To Purchase Charts Call 1-800-854-7179 USA Canada or 303-397-7956 Worl.pdf
《ANSI AWS D18.2-2009 GUIDE TO WELD DISCOLORATION LEVELS ON INSIDE OF AUSTENITIC STAINLESS STEEL TUBE (Abstract To Purchase Charts Call 1-800-854-7179 USA Canada or 303-397-7956 Worl.pdf》由会员分享,可在线阅读,更多相关《ANSI AWS D18.2-2009 GUIDE TO WELD DISCOLORATION LEVELS ON INSIDE OF AUSTENITIC STAINLESS STEEL TUBE (Abstract To Purchase Charts Call 1-800-854-7179 USA Canada or 303-397-7956 Worl.pdf(2页珍藏版)》请在麦多课文档分享上搜索。
1、AWS D18.2:2009An American National StandardAbstractThis standard addresses factors that affect weld discoloration on the inside of austenitic stainless steel tube. The documentcontains a color illustration relating the discoloration to the oxygen content of the backing shielding gas.Guide to Weld Di
2、scoloration Levels onInside of Austenitic Stainless Steel Tube1. This standard provides a visual comparison guide that can be used to specify surface discoloration criteria for sanitary(hygienic) welds in austenitic stainless steel tube.This figure has been extracted from AWS D18.1/D18.1M:2009.2. Th
3、e Tube Sample. The tube sample was prepared using an automatic orbital “bead-on-plate” weld on the outsidediameter of a 2 in 50.8 mm stainless steel tube. The weld penetrated through the tube wall. The concentration of oxygenin ppm added to the pure argon backing gas for each weld was as follows:No.
4、 110 ppm No. 350 ppm No. 5200 ppm No. 71000 ppm No. 912 500 ppmNo. 225 ppm No. 4100 ppm No. 6500 ppm No. 85000 ppm No. 1025 000 ppm3. The illustration is most useful as a reference to identify the degree of discoloration rather than to specify oxygenlimits in the backing gas. The amount of discolora
5、tion and its appearance can be influenced by factors other than oxygensuch as:High levels of moisture in the backing gas will increase the degree of discoloration.Contaminants such as hydrocarbons, moisture, and some types of particulate on the surface prior to welding caninfluence discoloration lev
6、els.Hydrogen gas in the argon backing gas can significantly reduce the amount of discoloration.The metals surface finish can affect the appearance of discoloration.No portion of this standard may be reproduced, stored in a retrieval system, or transmitted in any form, including mechanical, photo-cop
7、ying, recording, or otherwise, without the prior written permission of the copyright owner.Weld Discoloration Levels on Inside of Austenitic Stainless Steel Tube550 N.W. LeJeune Road, Miami, FL 33126Statement on the Use of AWS American National Standard StandardsAll standards (codes, specifications,
8、 recommended practices, methods, classifications, and guides) of the American Welding Society (AWS)are voluntary consensus standards that have been developed in accordance with the rules of the American National Standards Institute(ANSI). When AWS American National Standards are either incorporated
9、in, or made part of, documents that are included in federal or statelaws and regulations, or the regulations of other governmental bodies, their provisions carry the full legal authority of the statute. In suchcases, any changes in those AWS standards must be approved by the governmental body having
10、 statutory jurisdiction before they can becomea part of those laws and regulations. In all cases, these standards carry the full legal authority of the contract or other document that invokesthe AWS standards. Where this contractual relationship exists, changes in or deviations from requirements of
11、an AWS standard must be byagreement between the contracting parties.International Standard Book Number: 978-0-87171-756-6American Welding Society, 550 N.W. LeJeune Road, Miami, FL 33126 2009 by American Welding Society. All rights reserved.Printed in the United States of AmericaAWS American National
12、 Standards are developed through a consensus standards development process that brings together volunteers repre-senting varied viewpoints and interests to achieve consensus. While the AWS administers the process and establishes rules to promote fairnessin the development of consensus, it does not i
13、ndependently test, evaluate, or verify the accuracy of any information or the soundness of anyjudgments contained in its standards.AWS disclaims liability for any injury to persons or to property, or other damages of any nature whatsoever, whether special, indirect, con-sequential, or compensatory,
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
2000 积分 1人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- ANSIAWSD1822009GUIDETOWELDDISCOLORATIONLEVELSONINSIDEOFAUSTENITICSTAINLESSSTEELTUBEABSTRACTTOPURCHASECHARTSCALL18008547179USACANADAOR3033977956WORLPDF

链接地址:http://www.mydoc123.com/p-433898.html