PIA-C-3953F-2010 CLOTH DUCK NYLON《尼龙帆布》.pdf
《PIA-C-3953F-2010 CLOTH DUCK NYLON《尼龙帆布》.pdf》由会员分享,可在线阅读,更多相关《PIA-C-3953F-2010 CLOTH DUCK NYLON《尼龙帆布》.pdf(9页珍藏版)》请在麦多课文档分享上搜索。
1、 The following commercial specification is originally adopted from the military document. Revision A includes all known accepted revisions, amendments, notices, and Department of Defense (DoD) engineering changes previously developed for this item. Revisions B and forward include changes adopted by
2、DoD and Industry to reflect technology and design evolution. CLOTH, DUCK, NYLON The Parachute Industry Association makes this document available for use by Industry and Government organizations that wish to apply this specification to their products. 1. SCOPE 1.1 Scope. This specification covers nyl
3、on duck cloth. 1.2 ClassificationClass 1 - Untreated . The nylon duck cloth shall be of the following classes, as specified (see 6.1). Class 2 - Melamine resin treated (extra stiff) (0.45-0.65 pounds warp/0.65-0.85 pounds filling) Class 3 - Melamine resin treated (parachute procurement only) (0.3-0.
4、4 pounds warp/0.4-0.5 pounds filling) 2. APPLICABLE DOCUMENTS 2.1. General2.2 . The documents listed in this section are specified in Sections 3 and 4 of this specification. This section does not include documents cited in other sections of this specification nor is it recommended for additional inf
5、ormation or as examples. While every effort has been made to ensure the completeness of this list, document users are cautioned that they must meet all specified requirements of the documents cited in Sections 3 and 4 of this specification, whether or not they are listed. Government publications. 2.
6、2.1 Government publications. The following Government publications form a part of this document (see 2.4). STANDARDS FEDERAL FED-STD-4 - Glossary of Fabric Imperfections FED-STD-595 - Colors Used in Government Procurement PIA-C-3953F 17 November 2010 Superseding PIA-C-3953E 21 February 2009 DISTRIBU
7、TION STATEMENT: All Rights Reserved. No Part of this publication may be reproduced without prior written permission from the Parachute Industry Association. Additional copies may be purchased online from the PIA Store at: . PIA-C-3953F Page 2 of 9 (Unless otherwise indicated, copies of the above spe
8、cifications and standards are available from the Standardization Documents Order Desk, 700 Robbins Avenue, Building 4D, Philadelphia, PA 19111-5094. Electronic copies of Military and Federal standards and specifications may be obtained from https:/assist.daps.dla.mil/quicksearch/.) FEDERAL TRADE COM
9、MISSION (FTC) 16 CFR 303 - Rules and Regulations Under the Textile Fiber Products Identification Act (Copies are available online at: www.ftc.gov or from the Federal Trade Commission, 600 Pennsylvania Avenue, Washington, DC 20580-001. Electronic copies may be obtained from www.access.gpo.gov/.) 2.3
10、Non-government publications. The following documents form a part of this document. AMERICAN ASSOCIATION OF TEXTILE CHEMISTS AND COLORISTS (AATCC) AATCC-16 - Colorfastness to Light AATCC-61 - Colorfastness to Laundering: Accelerated AATCC-81 - pH of the Water-Extract from Wet Processed Textiles AATCC
11、-96 - Dimensional Changes in Commercial Laundering of Woven and Knitted Fabrics Except Wool AATCC Evaluation Procedures: - 1 Gray Scale for Color Change - 8 AATCC 9 -Step Chromatic Transference Scale - 9 Visual Assessment of Color Difference of Textiles (Applications for copies should be addressed t
12、o the AATCC National Headquarters, P.O. Box 12215, Research Triangle Park, NC 27709-2215. Electronic copies may be obtained from www.aatcc.org.) AMERICAN SOCIETY FOR QUALITY (ASQ) ANSI/ASQ Z1.4 - Sampling Procedures and Tables for Inspection by Attributes (Applications for copies should be addressed
13、 to American Society for Quality, 600 North Plankinton Avenue, Milwaukee, WI 53203. Electronic copies may be obtained from www.asq.org.) ASTM INTERNATIONAL (ASTM) ASTM D 276 - Standard Test Method for Identification of Fibers in Textiles ASTM D 1776 - Standard Practice for Conditioning and Testing T
14、extiles ASTM D 2261 - Standard Test Method for Tearing Strength of Fabrics by the Tongue (Single Rip) Procedure (Constant-Rate-of-Extension Tensile Testing Machine) PIA-C-3953F Page 3 of 9 ASTM D 3775 - Standard Test Method for Warp (End) and Filling (Pick) Count of Woven Fabrics ASTM D 3776 - Stand
15、ard Test Methods for Mass Per Unit Area (Weight) of Fabric ASTM D 5034 - Standard Test Method for Breaking Strength and Elongation of Textile Fabrics (Grab Test) (Application for copies should be addressed to the ASTM International, 100 Barr Harbor Drive, West Conshohocken, PA 19428-2959. Electronic
16、 copies may be obtained from www.astm.org.) PARACHUTE INDUSTRY ASSOCIATION (PIA) PIA-TEST METHOD-5202 - STIFFNESS OF CLOTH, DIRECTIONAL; CANTILEVER BENDING METHOD (Electronic copies may be obtained from .) 2.4 Revision levels of subsidiary documents. The documents listed in Section 2 shall be define
17、d as subsidiary documents, other Government documents, and non-government publications. Unless otherwise specified by the procuring activity, the revision level of subsidiary documents shall be the latest revision level as listed in the Acquisition Streaming and Standardization Information (ASSIST)
18、data base located at: https:/assist.daps.dla.mil/quicksearch/. 2.5 Order of precedence. In the event of a conflict between the text of this document and the references cited herein, the text of this document takes precedence. Nothing in this document, however, supersedes applicable laws and regulati
19、ons unless a specific exemption has been obtained. 3. REQUIREMENTS 3.1 Standard. The finished cloth shall match the standard for shade and appearance and shall be equal to or better than the standard with respect to all characteristics for which the standard is referenced (see 6.2). 3.2 Material3.2.
20、1 . Nylon. The nylon shall be a high tenacity bright nylon polyamide. The nylon shall be either Nylon 6 with a minimum melting point of 392F (203C) or Nylon 6,6 with a minimum melting point of 471F (244C) when tested as specified in 4.2.3. 3.3 Color. The color of the finished cloth shall be as speci
21、fied by the procuring activity (see 6.1). 3.3.1 Visual shade matching. If the fabric is dyed, the color of the dyed fabric shall match the standard when viewed using the AATCC Evaluation Procedure 9, Option A, with sources simulating artificial daylight D75 illuminate with color temperature of 7500
22、200K, illumination of 100 20 foot candles, and shall be a good match to the standard under incandescent lamplight at 2856 200k. PIA-C-3953F Page 4 of 9 3.3.2 Colorfastness. 3.3.2.1 Dyed fabric. If the fabric is dyed, the dyed fabric shall show fastness as follows: Characteristic Rating (minimum) Lig
23、ht (Fade) 1/3-4 Laundering 2/3-4 Notes: 1/Rated using the AATCC Evaluation Procedure 1, Gray Scale for Color Change 2/Rated using the AATCC Evaluation Procedure 1, Gray Scale for Color Change and AATCC Evaluation Procedure 2, Gray Scale for Staining. 3.4 Physical requirements. The cloth shall confor
24、m to the minimum requirements specified in TABLE I when tested as specified in 4.2.3. TABLE I Physical requirements 1/Weight oz./sq. yard (g/m2) Yarns per inch (cm) Breaking strength pounds (N) Tearing strength pounds (N) Warp Filling Warp Filling Warp Filling 18.5 1 62 60 1100 1100 135 135 (627 34)
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
10000 积分 0人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- PIAC3953F2010CLOTHDUCKNYLON 尼龙 帆布 PDF