《DLA A-A-59142-1998 ROSINS GUM WOOD AND TALL OIL [Superseded DLA LLL-R-626 D CANC NOTICE 2 DLA LLL-R-626 D VALID NOTICE 1 DLA LLL-R-626 D DLA LLL-R-626 C DLA LLL-R-626 B]《橡胶 木材和高油树脂.pdf》由会员分享,可在线阅读,更多相关《DLA A-A-59142-1998 ROSINS GUM WOOD AND TALL OIL [Superseded DLA LLL-R-626 D CANC NOTICE 2 DLA LLL-R-626 D VALID NOTICE 1 DLA LLL-R-626 D DLA LLL-R-626 C DLA LLL-R-626 B]《橡胶 木材和高油树脂.pdf(7页珍藏版)》请在麦多课文档分享上搜索。
1、 A-A-59142 = 974 0376742 543 = METRIC 21 Januarv 1998 SUPERSEDING 15 January 1991 A-A-59 142 LLL-R-626D COMMERCIAL, ITEM DESCRIPTION ROSINS: GUM, WOOD, AND TALL OIL The General Services Administration has authorized the use of this commercial item description for all federal agencies. 1. SCOPE. This
2、 commercial item description (CID) covers three classes, two types, and 13 grades of rosin. 2. CLASSIFICATION 2.1 Classes. Class A - Gum rosin (obtained fiom oleoresin collected fiom living trees). Class B - Wood rosin (obtained fiom the oleoresin contained in dead wood such as stumps and knots). Cl
3、ass C - Tall oil rosin (obtained fiom tall oil). 2.2 Tyves. Type I - Lump (solid mass (molten) or large lump) Type II - Powdered (ground fiom type I rosin) Beneficial comments, recommendations, additions, deletions, clarifications, etc., and any data which may improve this document should be sent by
4、 letter to: Defense Supply Center Richmond (DSCR), AT“: DSCR-VBD, 8000 Jefferson Davis Highway, Richmond, VA 23297-5610. AMSC N/A FSC 6810 DISTRIBUTION STATEMENT A. Approved for public release; distribution is unlimited. Provided by IHSNot for ResaleNo reproduction or networking permitted without li
5、cense from IHS-,-,-? A-A-59142 74 0176743 48T Requirement Except Grade FF As specified As specified 0.05 0.05 grade FF 2.3 Grades. Type I rosin shall be of the following grades as prescribed by the Naval Stores Act: ASTM test method D509 D269 Grade X (lightest color) Grade WW Grade WG Grade N Grade
6、M Grade K Grade I Grade H Grade G Grade F Grade E Grade D (darkest color) Grade FF (unrefined dark-colored wood rosin) 70 160 166 3. SALIENT CHARACTERISTICS. 67 150 162 3.1 Tvtie I rosin, physical and chemical characteristics shall conform to applicable physical and chemical characteristics of table
7、 I when tested as specified therein. TABLE I. Physical and chemical characteristics of tvrie I rosin. Characteristic Grade Insoluble matter in toluene, maximum percent by weight Softening point, OC, minimum Acid number, minimum Saponification number, minimum E28 D465 D464 3.2 TvDe II rosin. Dhvsical
8、 and chemical characteristics shall conform to applicable physical and chemical characteristics of table II when tested as specified therein. 3.2.1 Particle size. Weigh 100 f 1 g of the specimen into a large container and add approximately 1 liter of distilled water. Stir the rosin thoroughly in the
9、 water to separate all particles. Wash the rosin onto a 2.36 mm sieve conforming to ASTM El 1 with a gentle stream of water while gently brushing, with a camels hair brush, any matter retained on the sieve. No rosin shall remain on the sieve. 2 Provided by IHSNot for ResaleNo reproduction or network
10、ing permitted without license from IHS-,-,- A-A-59142 = 9999974 OI17b744 3Lb = Characteristic A-A-59 142 Requirement 3.2.2 Heat test. Weigh approximately 5 g of the specimen into a test tube and stopper lightly. Place the test tube in a water bath at 57 f 1C to the depth of the rosin in the test tub
11、e and let stand for 2 hours. Remove the test tube, wipe off the outside water, and gently tap with a pencil. Turn the contents out onto a sheet of paper or a flat dish. There shall be no aggregate lumps in the powdered material. Grade“ Insoluble matter in toluene, maximum percent by weight Softening
12、 point, OC, minimum“ Acid number, minimum” Saponification number, minimum() Particle size Heat test TABLE II. Physical and chemical characteristics of twe II rosin. All grades except FF As specified 10.0 70 160 166 100% pass 2.36 mm sieve Uncongealed and free from lumps Grade-FF As specified 10.0 67
13、 150 1 62 100% pass 2.36 mm sieve Uncongealed and free from re grinding. lumps ASTM test method D509 D269 E28 D465 D464 3.2.1 3.2.2 4. REGULATORY REQUIREMENTS. 4.1 Recovered materials. The offerorkonactor is encouraged to use recovered materials to the maximum extent practicable, in accordance with
14、paragraph 23.403 of the Federal Acquisition Regulation (FAR). Unless otherwise specified herein, all equipment, material, and articles incorporated in the work covered by this commercial item description are to be new and fabricated using materials produced from recovered materials to the maximum ex
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
10000 积分 0人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- DLAAA591421998ROSINSGUMWOODANDTALLOILSUPERSEDEDDLALLLR626DCANCNOTICE2DLALLLR626DVALIDNOTICE1DLALLLR626DDLALLLR626CDLALLLR626B

链接地址:http://www.mydoc123.com/p-687106.html