1、 GMDAT ENGINEERING STANDARDS Material Specification Plastics EDS-M-4102 Linear Low Density Polyethylene Copyright 2010 General Motors All Rights Reserved April 2010 Originating Department: GMDAT Engineering Standards Page 1 of 4 Version : 8 1 Scope Note: Nothing in this standard supersedes applicabl
2、e laws and regulations. Note: In the event of conflict between the Korean and English language, the Korean language shall take precedence. 1.1 Material Description. Raw materials that have excellent impact strength and good processability. 1.1.1 Material Types. 1.1.1.1 Type 1. Ex) Protecting cap. 1.
3、1.1.2 Type 2. Ex) Energy absorber. 1.2 Symbols. Material indication: PE -LLD PE -LLD. ( : GMW3116) . 1.3 . (LINEAR LOW DENSITY POLYETHYLENE) . 1.4 . 2 / : . 2.1 / . . 2.2 GM / . EDS-M-0102 EDS-T-7504 EDS-T-7511 EDS-T-7516 EDS-T-7518 EDS-T-7520 GMW 3059 EDS-T-7406 EDS-T-7510 EDS-T-7514 EDS-T-7517 EDS
4、-T-7519 GMW3001 GMW 3116 2.3 / . . GMDAT ENGINEERING STANDARDS EDS-M-4102 Copyright 2010 General Motors All Rights Reserved April 2010 Page 2 of 4Version : 8 3 Requirements 3.1 Mechanical properties. 3 3.1 . Table 1: Mechanical Properties / 1: Properties / Type 1 / 1 Type 2 / 2 Rockwell hardness / E
5、DS-T-7517 R Scale 50 50 Tensile strength (kg/cm2) / (kg/cm2) EDS-T-7511 Test piece (63 mm) / (63 mm) Test speed (50 mm/min) / (50 mm/min) 150 150 Elongation (%) / (%) EDS-T-7511 Test piece (63 mm) / (63 mm) Test speed (50 mm/min) / (50 mm/min) 500 400 Flexural strength (kg/cm2) / (kg/cm2) EDS-T-7518
6、 Test piece (12712.76.4 mm) / (12712.76.4 mm) Test speed (28 mm/min) / (28 mm/min) - - Flexural modulus (kg/cm2) / (kg/cm2) EDS-T-7510 Test piece (12712.76.4 mm) / (12712.76.4 mm) Test speed (28 mm/min) / (28 mm/min) 2,000 1,500 Impact strength, IZOD (kg cm/cm) / IZOD (kg cm/cm) EDS-T-7514 Test piec
7、e (63.512.73.2 mm) / (63.512.73.2 mm). Room temperature / -30 NB - NB - 3.2 Thermal Properties. 3.2 . Table 2: Thermal Properties / 2: Properties / Type 1 / 1 Type 2 / 2 Melting point ( ) / ( ) EDS-T-7519 105 105 Heat deflection temperature ( ) / ( ) EDS-T-7520 Test piece (127 12.7 6.4mm) / (12712.7
8、6.4mm) 4.6 kg/cm2- - GMDAT ENGINEERING STANDARDS EDS-M-4102 Copyright 2010 General Motors All Rights Reserved April 2010 Page 3 of 4Version : 8 Properties / Type 1 / 1 Type 2 / 2 VICAT softening point ( ) / VICAT ( ) EDS-T-7504 1 kg 95 90 3.3 General Properties. 3.3 . Table 3: General Properties / 3
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
10000 积分 0人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- GMKOREAEDSM41022010LINEARLOWDENSITYPOLYETHYLENEVERSION8ENGLISHKOREANPDF

链接地址:http://www.mydoc123.com/p-756641.html