FORD WSB-M11P41-B1-2013 ADHESIVE REQUIREMENTS EXTERIOR REAR VIEW MIRROR ASSEMBLY TO BE USED WITH FORD WSS-M99P1111-A .pdf
《FORD WSB-M11P41-B1-2013 ADHESIVE REQUIREMENTS EXTERIOR REAR VIEW MIRROR ASSEMBLY TO BE USED WITH FORD WSS-M99P1111-A .pdf》由会员分享,可在线阅读,更多相关《FORD WSB-M11P41-B1-2013 ADHESIVE REQUIREMENTS EXTERIOR REAR VIEW MIRROR ASSEMBLY TO BE USED WITH FORD WSS-M99P1111-A .pdf(4页珍藏版)》请在麦多课文档分享上搜索。
1、 ENGINEERING MATERIAL SPECIFICATIONMaterial Name Specification NumberDate Release No. Release/Revision1991 02 01 C01089481000 Released W. Scholz Conc. J. SchultWP 3948-a Page 1 of 4 ADHESIVE REQUIREMENTS, EXTERIOR REAR VIEW WSB-M11P41-B1MIRROR ASSEMBLY1. SCOPEThis specification defines the performan
2、ce requirements for an adhesive oran adhesive system for bonding glass to liner and liner to shell inexterior rear view mirror assembly.2. APPLICATIONThi s specification was released originally for adhesives used to bondglass, plastic, stainless steel, and phosphated galvanized steel.Compl iance wit
3、h this performance specification does not guarantee theadhesiv e will function for all potential applications on a vehicle. Thespe cific assembly should be evaluated to design engineering performancerequirements.3. REQUIREMENTS3.1 STATISTICAL PROCESSSupplie rs must conform to the requirements of For
4、d Quality SystemStand ard Q-101. A mutually acceptable Control Plan as describedtherein is required for material/source approval. Appropriatestatist ical tools must be used to analyze process/product data sothat variation in the final product is continuously reduced.3.2 INFRARED SPECTROPHOTOMETRY AN
5、D/OR THERMAL ANALYSISFord Motor Company, at its option, may conduct infrared and/ortherma l analysis of material/parts supplied to this specification.The IR spectra and thermograms established for i nitial approval shallconst itute the reference standard and shall be kept on file at thedesignated ma
6、terial laboratory. All samples sha ll produce IR spectraand thermograms that correspond to the reference standard when testedunder the same conditions.3.3 CONDITIONING AND TEST CONDITIONSAll test values indicated herein are based on materials conditionedin a co ntrolled atmosphere of 23 +/- 2 C and
7、50 +/- 5 % relativehumidity for not less than 24 h prior to testing and tested under thesame conditions unless otherwise specified.ENGINEERING MATERIAL SPECIFICATIONWSB-M11P41-B1WP 3948-b Page 2 of 4 3.4 SHEAR ADHESION, min(SAE J1523, 0.76 mm bondline thickness, 25 mm bondoverlap, 50 mm/minute pull
8、rate, substrates perpara 5.1, three samples min per test condition,pre-condition bonded samples 72 h at 23 +/- 2 C)Normal(Condition for 30 minutes at specified temperature prior to test)3.4.1 Test at 23 +/- 2 C 690 kPa3.4.2 Test at - 30 +/- 2 C 830 kPaEnvironmental Age(Condition at 23 +/- 2 C for 24
9、 h afterexposure, then test at 23 +/- 2 C)3.4.3 336 h at 90 +/- 2 C 690 kPa3.4.4 30 minutes at 120 +/- 2 C 690 kPa3.4.5 120 h deionized water immersion at 410 kPa60 +/- 2 C3.4.6 5 cycles with each of the following: 690 kPa. 4 h at 90 +/- 2 C. 4 h at 38 +/- 2 C and 95-100 % R.H. 16 h at - 30 +/- 2 C.
10、 4 h at 38 +/- 2 C and 95-100 % R.H. 4 h at 90 +/- 2 C. 16 h at - 30 +/- 2 C(Maintain sample at - 30 +/- 2 C over weekend)3.4.7 260 kJ/m2 Xenon Arc Exposure per 690 kPa(SAE J1960, Glass test samples only)3.5 NON-CORROSIVE PROPERTIES No CorrosionTest Method: Extrude 15 g of material into a cr ucible
- 1.请仔细阅读文档,确保文档完整性,对于不预览、不比对内容而直接下载带来的问题本站不予受理。
- 2.下载的文档,不会出现我们的网址水印。
- 3、该文档所得收入(下载+内容+预览)归上传者、原创作者;如果您是本文档原作者,请点此认领!既往收益都归您。
下载文档到电脑,查找使用更方便
10000 积分 0人已下载
下载 | 加入VIP,交流精品资源 |
- 配套讲稿:
如PPT文件的首页显示word图标,表示该PPT已包含配套word讲稿。双击word图标可打开word文档。
- 特殊限制:
部分文档作品中含有的国旗、国徽等图片,仅作为作品整体效果示例展示,禁止商用。设计者仅对作品中独创性部分享有著作权。
- 关 键 词:
- FORDWSBM11P41B12013ADHESIVEREQUIREMENTSEXTERIORREARVIEWMIRRORASSEMBLYTOBEUSEDWITHFORDWSSM99P1111APDF

链接地址:http://www.mydoc123.com/p-748866.html